[1]李权,林金国,齐文玉,等.3 种木材涂饰前后表面视觉性质差异的研究[J].浙江林业科技,2017,37(05):66-68.[doi:10.3969/j.issn.1001-3776.2017.05.011]
 LI Quan,LIN Jin-guo,QI Wen-yu,et al.Differences of Surface Visual Physics Magniture of Three Kinds of Timber Before and After Painting[J].Journal of Zhejiang Forestry Science and Technology,2017,37(05):66-68.[doi:10.3969/j.issn.1001-3776.2017.05.011]
点击复制

3 种木材涂饰前后表面视觉性质差异的研究()
分享到:

《浙江林业科技》[ISSN:1001-3776/CN:33-1112/S]

卷:
37
期数:
2017年05期
页码:
66-68
栏目:
研究简报
出版日期:
2017-11-30

文章信息/Info

Title:
Differences of Surface Visual Physics Magniture of Three Kinds of Timber Before and After Painting
作者:
李权12林金国2齐文玉2柯丽丽2林加志2
1. 凯里学院,贵州 凯里 556011;2. 福建农林大学 材料工程学院,福建 福州 350002
Author(s):
LI Quan12LIN Jin-guo2QI Wen-yu2KE Li-li2LIN Jia-zhi2
1. Kaili University of Guizhou, Kaili 556011, China; 2. College of Material Engineering, Fujian Agriculture and Forestry University, Fuzhou350002, China
关键词:
筒状非洲楝古夷苏木水曲柳醇酸清漆涂饰木材表面视觉性质
Keywords:
Entandrophragma cylindricum Guibourtia tessmannii Fraxinus mandschurica alkyd varnish painting wood surface visual physicsmagnitude
分类号:
S781
DOI:
10.3969/j.issn.1001-3776.2017.05.011
文献标志码:
A
摘要:
测定分析了筒状非洲楝Entandrophragma cylindricum,古夷苏木Guibourtia tessmannii 和水曲柳Fraxinusmandschurica 木材醇酸清漆涂饰前后表面视觉性质的差异。结果表明,涂饰处理降低了3 种木材表面的明度(L*)和红绿轴色品指数(a*)值,其中,古夷苏木的L*变化差异最大,明度降低明显;水曲柳的红绿轴色品指数差(Δa*)绝对值最大,相比处理前更偏向绿色;3 种木材透明涂饰后的黄蓝轴色品指数(b*)均有所升高,黄蓝轴色品指数差(Δb*)绝对值由大到小分别为水曲柳>古夷苏木>筒状非洲楝,数值越大越趋于黄色;总体色差(ΔE*)变化差异不大,涂饰对3 种木材的总体色差影响不明显。
Abstract:
Determinations were conducted on visual physics magnitude of Entandrophragma cylindricum, Guibourtia tessmannii and Fraxinusmandschurica wood before and after painting alkyd varnish. The results show that painting reduced the luminance (L*) and the chrominance (a*) oftested wood specimen, the biggest change L* was specimen of G. tessmannii wood with obvious decrease of luminance. The absolute value (Δa*) ofF. mandschurica wood was the largest, greener than that of untreated one. The chrominace (b*) of three kinds of wood specimen increased afterpainting, and the absolute Δb* was ordered by specimen of F.mandschurica > G. tessmannii > E. cylindricum. Chrominance aberration (ΔE*) oftested wood specimen had little difference before and after painting.

参考文献/References:

[1] 罗玉华,朱林峰,刘元,等. 巨桉不同家系木材表面视觉性质的研究[J]. 林业科技开发,2005,19(2):26-28.
[2] 朱林峰,刘元,罗玉华,等. 粗皮桉不同家系木材的表面视觉性质[J]. 中南林业科技大学学报,2004,24(4):41-46.
[3] Bulian F,Graystone J A. Wood Coating: Theory and Practice[C]. Internationale Deutschlehrerinnen Tagung. Bull Fed Soc Gynecol Obstet LangFr,2009.
[4] Bessières J,Maurin V,George B,et al. Wood-coating layer studies by X-ray imaging[J]. Wood Sci Technol,2013,47(47):853-867.
[5] 刘一星,李坚,于晶,等. 透明涂饰处理前后木材表面材色和光泽度的变化[J]. 家具,1995(3):3-5.
[6] 侯新毅,姜笑梅,殷亚方. 从色度学参数研究3 种桉树木材的透明涂饰性能[J]. 林业科学,2006,42(8):57-62.
[7] 梁善庆,彭立民,傅峰. 五种珍贵木材涂饰色度学变化及性能评价[J]. 木材加工机械,2014(3):16-21.
[8] 李坚,刘一星,方桂珍. 木材表面视觉环境学特性分析Ⅱ.木材视觉心理量的解析[J]. 木材工业,1995(3):20-23.
[9] 佐道健. 机器に ょる测定值か ら视觉值へ の换算:L*、a*、b*表色系か ら マ ソ セ へ の变换[J]. 木材工业,1985(1):12-40.
[10] 刘宏达,高建民,陈瑶. 预热处理对改善尾巨桉木材干缩性和材色的研究[J]. 西北林学院学报,2014,29(5):176-180.
[11] 曹积微,袁哲,强明礼. 微波和汽蒸加热软化棕榈藤材抗弯性能及材色的比较研究[J]. 西南林业大学学报,2016,36(4).
[12] 鲍甫成,王正,郭文静. 杨木和杉木木材表面性质的研究[J]. 林业科学,2004,40(1):131-136.
[13] 胡吉萍. 福建四种实木家具用材涂饰性能的研究[D]. 福州:福建农林大学,2013.
[14] 侯新毅. 三种桉树木材的机械加工和透明涂饰性能研究[D]. 北京:北京林业大学,2004.
[15] 常德龙,张云岭,马志刚,等. 泡桐材墙壁板两种涂饰工艺效果差异[J]. 东北林业大学学报,2015(2):116-118.

备注/Memo

备注/Memo:
收稿日期:2017-06-03 ;修回日期:2017-08-22基金项目:国家自然科学基金项目(31760191);福建省财政厅科研基金资助项目“进口木材特性与鉴别关键技术研究与推广”(K8115004A);贵州省高校优秀科技创新人才奖励计划(黔教合KY 字﹝2015﹞508)作者简介:李权,副教授,博士,从事木结构建筑以及木材防腐技术研究;E-mail:liquan-8@163.com。通信作者:林金国,教授,博士生导师,从事木材科学研究;E-mail:fjlinjg@126.com。
更新日期/Last Update: 2017-10-20